Step in Solvent removable method.

5. Inspection:

Inspection  with visible dye penetrant  with minimum whate light intensity 100 foot-candles or 1100 lux  shall follow. Ultraviolet (UV-A) radiation of minimum intensity 1,000 micro-watts per centimeter squared is common, along with low ambient light levels (less than 2 foot-candles) for fluorescent penetrant examinations. Inspection of the test surface should take place after 10- to 30-minute development time, and is dependent on the penetrant and developer used. This time delay allows the blotting action to occur. The inspector may observe the sample for indication formation when using visible dye. It is also good practice to observe indications as they form because the characteristics of the bleed out are a significant part of interpretation characterization of flaws.

6. Post Cleaning:

The test surface is often cleaned after inspection and recording of defects, especially if post-inspection coating processes are recommended as per PT procedure.

Leave a Reply

Fill in your details below or click an icon to log in:

WordPress.com Logo

You are commenting using your WordPress.com account. Log Out /  Change )

Twitter picture

You are commenting using your Twitter account. Log Out /  Change )

Facebook photo

You are commenting using your Facebook account. Log Out /  Change )

Connecting to %s